Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Vibration plate dimension (mm) and instrumentation locations Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Vibratory analysis of the chordwise mode on a square plate: (a) von Mises stress and (b) mode shape Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Dogbone cutout orientation is used to separate the multiple sentences Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / (a) DMLS build direction schematic and (b) top view of build structure Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Point cloud mesh to CAD geometry comparison: (a) cold-rolled and (b) specimen #7 DMLS before milling Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Forced response strain amplitude versus shaker head acceleration during sweeps: specimen #7 Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Forced response quality factor versus shaker head acceleration during sweeps: specimen #7 Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Ti 6Al–4V vibration bending fatigue life comparison Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Comparison of ultimate tensile strength deviation from population per fatigue plate Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / Fractograph of DMLS specimen #1 Figure Legend:
Date of download: 6/23/2016 Copyright © ASME. All rights reserved. From: Fatigue and Strength Studies of Titanium 6Al–4V Fabricated by Direct Metal Laser Sintering J. Eng. Gas Turbines Power. 2015;138(2): doi: / SEM micrographs of Ti 6Al–4V: (a) DMLS and (b) cold-rolled Figure Legend: