Centrifugal Casting of Microfluidic Components With PDMS Date of download: 10/1/2017 Copyright © ASME. All rights reserved. Centrifugal Casting of Microfluidic Components With PDMS J. Micro Nano-Manuf. 2013;1(2):021001-021001-8. doi:10.1115/1.4023754 Figure Legend: (a) Heating and cooling station for curing PDMS in a mold assembly for centrifugal casting. The total height of the system is 91 cm. (b) Ceramic heaters on a pneumatic cylinder rise to make contact with the bottom of the mold and heat the mold assembly for 4 min. (c) After heating the PDMS is complete, a set of chilled blocks come down from the top to cool the mold for 4 min.