Zircon crown Kristýna dandová
Situational model
Tooth 23 is going to be restored by zircon crown
Creating of zircon framework
Zircon block InLab program
The process of milling
Milling
Regeneration firing
Zircone building For building of the crown was used Ivoclar vivadent IPS e.max systém
Zir Liner Creates connection between framework and e.max mass ZirLiner ( powder+ liquid) has to be applied over whole surface by protracted movements
Firing - 960°C for 1 min
Building of the crown Building starts with aplying of Dentin. The mass is applied by special brush for ceramics
Firing - 750°C for 1 min
Building of the crown Building of the crown continues with applying of Transpa inscisal The crown is builded into approximate shape of tooth
The crown after second firing
Machining Process of machining Neck Contact Height ( articulation) Morfology Surface texture
Glaze For glazing of the crown was used IPS Empress
Firing - 725° for 1min 30 sec
Final version