GE Water & Process Technologies Korea “H” Paper Petrocoke Boiler Furnace Slagging Comparison (CEC2571 TEST RESULT) GE Water & Process Technologies Korea
Test Summary Fuel Type: Petro coke Test Period - Before CEC2571: 30 days - After CEC2571: 2011. 07.15~08. 09(25 days) TEST Result - Before using CEC2571 (actually treated by other vendor’s MgO product), the slagging and fouling material nearly blocked the gas passages of tubes. Also, the slagging was so hard to remove during shutdowns. - After using CEC2571, the slagging and fouling was significantly reduced. Also, the slagging was soft and easy to remove during a shutdown. - The boiler system is operating for more than 10 months without plant shutdown.
Before/After Furnace Photo 1 Riser Tubes: Blocked by slagging Riser Tubes : No blocking
Before/After Furnace Photo 2 Middle Part: Blocked by slagging Middle Part: No blocking and clean
Before/After Furnace Photo 3 Upper part: Blocked by slagging Upper part: Significantly reduced in slagging
Before/After Furnace Photo 4 Bottom: Heavy slagging Bottom : Significantly reduced in slagging