Diffusers – Ni Resist Refurbished Vane Cracks
3
Discharge Bowl – Ni Resist Web Cracks
4
Outer Columns – Ni Resist Cracks
5
Spiders – Ni-Resist
6
Stuffing Box – Cast Iron New Severe corrosion presumed caused by galvanic difference between cast iron stuffing box and stainless enclosing tube.
7
Shaft – Nitronic 50 Shaft material in good shape. Wear is at bearings due to misalignments, imbalances, etc.
8
Impellers– Stainless Steel Enclosing Tube – Nitronic 50 (SS) 300 series stainless steel parts are in good condition. (these are not new)