SJVRWRF Dewatering Building Corrosion Remediation
Marc Serna, P.E. September 28, 2017
2
SJVRWRF Dewatering Building Corrosion Remediation
Dewatering Building Roof Plan Building was built in It is made of block wall with roof metal deck at 22-ft above floor with work area of 4,200-sq.ft Contractor scope-of-work is to re-coat existing roof structural supports and metal decking. Existing coating contains lead. Contractor to protect and allow operation of dewatering equipment during construction. LIMIT OF WORK EXTENT OF PLATFORM / DECKING INSTALLED BY CONTRACTOR EXTENT OF SURFACE PREPARED BY CONTRACTOR
3
Metal Decking and Structural Support Condition
SIGNS OF CORROSION ON STRUCTURAL SUPPORT BEFORE PARTICLE BLASTING SIGNS OF CORROSION METAL DECKING BEFORE PARTICLE BLASTING
4
Metal Decking After Particle Blasting
TEST AREA: METAL DECKING AFTER PARTICLE BLASTING
5
After Inspection of Applied Epoxy Primer
TEST AREA: AFTER SCRAPING OF LIFTED MATERIALS (PUTTY KNIFE TEST FOR ADHESION)
6
Metal Decking after 1st Layer Epoxy Primer Application
TEST AREA: METAL DECKING AFTER 1ST LAYER EPOXY PRIMER COATING AFTER REMOVING ACRYLIC COATING
7
Beams after 1st Layer Primer Application
STRUCTURAL SUPPORT AFTER PARTICLE BLASTING AND 1ST LAYER EPOXY PRIMER APPLICATION
8
Recommendations Staff recommends 100% removal of acrylic including old primer with lead. Approve and authorize amendment to agreement with Schuler Constructors for an amount of $83,800. Additional appropriation of $125,600 to fund the balance of the change order and expenses through the construction phase of the project for a total project cost of $398,300.
9