Cold process: used at room temperature, no stress or adjustments because of termal distorsion. To tolerance: normaly no machining required Quick metal build-up: 0,05 mm in min. Plating: on all conductive materials, cast iron, stainless, mild steel, copper, chrome etc Dense deposits: no or very little porosity in most coatings Many differens metals: nickel, gold, silver, copper, cobolt, zinc and alloys. Excellent bonding: molecular bonding results in very god adhesion, all coatings can be machined, ground or polished. Mobile equipment: the repair can be done on site

4 LDC borstplätering Retainingrings, part of generator for powerstation, silverplated.

5 LDC borstplätering Retainingrings, part of generator for powerstation, silverplated.

6 LDC borstplätering Bus bar, contact rods for the power generating industry, gold and silver coated contact-surfaces for increased conductivity.

7 LDC borstplätering On-site plating job, shafts to be restored

8 LDC borstplätering Electric rotor with bad / worn bearing / seal areas repaired to original size.

9 LDC borstplätering Electric rotor with bad / worn bearing / seal areas repaired to original size.

10 LDC borstplätering Endcover of cast iron or Aluminium with worn /mismachined bearing seat corrected by LDC nickel.

11 LDC borstplätering Worn shaft on a turbine wing in power plant, to be repaired.

12 LDC borstplätering Tel: +46 248 17440 ldc@swipnet.se
Onsite repair of 2  pieces of seal  surfaces on a compressor  shaft due to  local wear damage. Built with the LDC-2904 Copper Hi-speed 0.5 mm.

13 LDC borstplätering Tel: +46 248 17440 ldc@swipnet.se
Finished compressor  shaft to its original dimensions,  with a hard, dense  top layer of the LDC-2874 Nickel Tungsten. With a hardness of 58 Hrc

14 LDC borstplätering Bearing journals and sealareas can be repaired on a Turboshaft Highly polished cylinders with damages is corrected by LDC plating

15 Propellershaft sleeve repaired on-site in England by LDC
LDC borstplätering Propellershaft sleeve repaired on-site in England by LDC

16 LDC borstplätering Documented view of enlarged LDC-2807 Nickel layer, as part of quality control.

17 LDC borstplätering Typical document of approval for LDC in Sweden.