Download presentation
Presentation is loading. Please wait.
1
Merlin Resilient even under Extreme Vibration
Merlin virtually eliminates the impact of cell cracks & ribbon fatigue. Extreme Vibration (Customer Field test) Merlin Panel Standard Bus Bar Merlin < 0.5% Standard > 30% Energy Efficiency Drop
2
Merlin Module >50X Durable in Thermal Cycling
-70C to +85C Thermal/Temperature Cycling
3
Merlin Module Resilient Despite Extreme Cell Cracking
PRE-TEST POST TEST Isc Voc FF Power (max) PRE 9.098 3.809 0.775 26.852 POST 8.746 3.662 0.640 20.508 % drop 3.87% 17.36% 23.63%
4
Merlin Module Resilient Despite Extreme Cell Cracking
PRE Solar Panel was attached to the standing seam roof pane and sent through the roll forming tool POST ~90% Power Output in-spite of severe damage!!!
Similar presentations
© 2025 SlidePlayer.com. Inc.
All rights reserved.