Rigid Pavement Concrete. Transverse Cracking Rigid Pavement Transverse Cracking Causes:  Slab longer than 15’ Slab Curl Curing.

Similar presentations


Presentation on theme: "Rigid Pavement Concrete. Transverse Cracking Rigid Pavement Transverse Cracking Causes:  Slab longer than 15’ Slab Curl Curing."— Presentation transcript:

1 Rigid Pavement Concrete

2 Transverse Cracking

3 Rigid Pavement Transverse Cracking Causes:  Slab longer than 15’ Slab Curl Curing

4 Rigid Pavement Transverse Cracking Causes:  Slab longer than 15’ Slab Curl Curing

5 Rigid Pavement Transverse Cracking Causes:  Slab longer than 15’ Slab Curl Curing

6 Rigid Pavement Transverse Cracking Cures:  Crack Sealing  Full-depth rigid repair  Dowel bar retrofit

7 Rigid Pavement Longitudinal Cracking

8 Rigid Pavement Longitudinal Cracking Causes:  Waiting too long to cut center joint

9 Rigid Pavement Longitudinal Cracking Causes:  Waiting too long to cut center joint  Subsoil settlement

10 Rigid Pavement Longitudinal Cracking Causes:  Waiting too long to cut center joint  Subsoil settlement

11 Rigid Pavement Longitudinal Cracking Causes:  Waiting too long to cut center joint  Subsoil settlement Meander cracks

12 Rigid Pavement Longitudinal Cracking Cures  Joint Sealing  Full Depth replacement  Subsurface stabilization

13 Rigid Pavement Pumping

14 Pumping Causes:  Water  Fines  Lack of load transfer  Loading

15 Rigid Pavement Pumping Causes:  Water  Fines  Lack of load transfer  Loading

16 Rigid Pavement Pumping Causes:  Water  Fines  Lack of load transfer  Loading

17 Rigid Pavement Pumping Cures  Under sealing  Dowel bar retrofit  Full depth rigid repair  Concrete pavement grinding

18 Rigid Pavement Faulting

19 Faulting Causes:  End-result of pumping

20 Rigid Pavement Faulting Causes:  End-result of pumping  Eroded subsoil

21 Rigid Pavement Faulting Causes:  End-result of pumping  Eroded subsoil

22 Rigid Pavement Faulting Cures:  Full-depth rigid repair  Undersealing  Dowel bar retrofit  Grinding

23 Rigid Pavement Transverse Joint Spalling

24 Rigid Pavement Transverse Joint Spalling Causes:  Improper dowel alignment

25 Rigid Pavement Transverse Joint Spalling Causes:  Improper dowel alignment  Lack of joint seal

26 Rigid Pavement Transverse Joint Spalling Causes:  Improper dowel alignment  Lack of joint seal  Incompressible s in joint

27 Rigid Pavement Transverse Joint Spalling Cures:  Crack & Joint Seal  Bonded Patching  Full-depth patching

28 Rigid Pavement Wear & Polishing

29 Rigid Pavement Wear & Polishing Causes:  Traffic wears off surface aggregate

30 Rigid Pavement Wear & Polishing Cures:  Grinding  Asphalt Overlay

31 Rigid Pavement Scaling

32 Scaling Causes:  Non-air- entrained concrete

33 Rigid Pavement Scaling Causes:  Non-air- entrained concrete  De-icing chemicals

34 Rigid Pavement Scaling Causes:  Non-air- entrained concrete  De-icing chemicals  Improper finishing technique

35 Rigid Pavement Scaling Cures:  Grinding  Asphalt overlay  Bonded resurfacing  Partial depth patch

36 Rigid Pavement Shallow Reinforcing

37 Rigid Pavement Shallow Reinforcing Cause:  Reinforcing Steel too close to surface

38 Rigid Pavement Shallow Reinforcing Cause:  Reinforcing Steel too close to surface

39 Rigid Pavement Shallow Reinforcing Cure:  Asphalt overlay or patch  Replacing steel & partial or full depth repair

40 Rigid Pavement D-Cracking

41 D-Cracking Causes:  Poor quality aggregate

42 Rigid Pavement D-Cracking Causes:  Poor quality aggregate  Freeze/thaw cycle

43 Rigid Pavement D-Cracking Cures:  Temporary: Partial depth asphalt patch  Permanent: Full-depth repair

44 Rigid Pavement Corner Cracking

45 Rigid Pavement Corner Cracking Causes:  Insufficient soil support

46 Rigid Pavement Corner Cracking Causes:  Insufficient soil support  Temperature related slab movement

47 Rigid Pavement Corner Cracking Cures:  Partial or full- depth patch  Replace slab  Stabilize subsurface

48 Rigid Pavement Blowups

49 Blowups Causes:  Expansion of concrete

50 Rigid Pavement Blowups Causes:  Expansion of concrete  Poorly sealed joints

51 Rigid Pavement Blowups Causes:  Expansion of concrete  Poorly sealed joints  Hot weather

52 Rigid Pavement Blowups Cures:  Pressure relief joints to prevent  Patch or reconstruction after occurrence