TM Proper Elastomeric Seal Selection for Process Analyzer Sample Systems Steve Doe Parker Hannifin Corporation
2
TM Topics Elastomeric Seals & NeSSI Compounding O-Ring Design Chemical Compatibility Proper Elastomeric Seal Selection for Process Analyzer Sample Systems
3
TM No Matter Which System... Elastomeric Seals & NeSSI
4
TM Elastomeric Seals & NeSSI …Elastomeric Seals Are In The Picture!
5
TM Elastomeric Seals & NeSSI Seal Do’s & Don’ts Do: “Capture” IntraFlow Pressure Connector R-Max Surface Mount Interface (not SP76) SP76 Interface Don’t: Expose Seal ID to Fluid Flow
6
TM Metal and plastic retained elastomeric composite seals Polymeric and plastic seals Homogeneous and inserted elastomeric shapes Elastomeric O-Rings Rubber and plastic boots/bellows Extruded and precision-cut and fabricated elastomeric seals Thermoplastic engineered seals EMI shielding and thermal management products Seal Group Products
7
TM Elastomeric Seals & NeSSI Alternatives: Special Geometry O-Ring Seal Special Geometry O-Ring Seal Mold Onto Stainless Wafer Mold Onto Stainless Wafer Stick With 2-007 in Couterbore (what we have) Stick With 2-007 in Couterbore (what we have)
8
TM “… designs and manufactures engineered elastomeric o-ring seals.” Parker O-Ring Division
9
TM Extrusion & Nibbling Failure Modes Spiral Failure Explosive Decompression Cutting
10
TM The seal swells, shrinks, loses physical properties, or gets brittle. Excessive swell, brittleness, and dramatic loss in physical properties Shrinkage: the fluid is extracting something from the rubber (changing the base polymer usually isn’t required.) Failure Modes Chemical Attack
11
TM Butyl (IIR) Neoprene (CR) Ethylene-Propylene (EPR, EPDM) Fluorosilicone (FVMQ) Nitrile (NBR) Polyacrylate (ACM) Hydrogenated Nitrile (HNBR) Polyurethane (AU, EU) Silicone (VMQ) Fluorocarbon (FKM) Tetrafluoroethylene- Propylene (TFE/P) Perfluoroelastomer (FFKM) O-Ring Polymers
12
TM GLT V0835-75 A V1164-75 B V0834-75 GF V0965-80 GFLT V1163-75 Extreme V1260-75 Hifluor V3819-75 Parofluor TM V8545-75 NEW V1263-75 Performance of Fluorocarbon
13
TM Performance of Fluorocarbon
14
TM Parofluor is a true Perfluoroelastomer polymer The Parofluor base polymer is a composition of 3 or more monomers A & B represent different fillers and curatives used to enhance physical & thermal properties Parofluor™ Ultra
15
TM to 550to 6005 to 4465 to 6085 to 525Temperature Range, F 3525 1619 Compression Set, 70 hrs at 400F, % (2-214 O-rings) --+5 +6TR – 10, F 125150140124135Elongation, % 18001050115011311262Modulus at 100%, psi 27002450175017402045Tensile Strength, psi 8075 Durometer, Shore A Kalrez 1050 Kalrez 4079 Chemraz 505 FF200-75FF500-75Physical Properties to 527 30 - 160 1050 2200 75 Kalrez 6375 Parofluor™ Ultra
16
TM Parofluor™ Ultra
17
TM Base polymer determines chemical resistance, rough temperature limits, and rebound resilience In some materials, the high and low temp limits can be modified by other compounding ingredients. Provides “baseline” for abrasion resistance, compression set resistance, permeability These can (and almost always are) modified – up or down – by other compounding ingredients. Compounding: Polymer Selection
18
TM Polymer chains must be cross-linked to achieve resilience and elasticity. Sulfur Organic Peroxides Bisphenol Others: specialty materials have special cure chemistry Compounding: Cure Systems
19
TM Reinforcing agents add mechanical strength and resistance to abrasion & permeation Carbon black: standard for black compounds Silica: standard for non-black compounds Fillers lower the cost of a compound but reduce compression set resistance and elongation Compounding: Fillers
20
TM Oils and / or polymers to lower the low temp limits and make the material flow better Reduce resistance to compression set In “generic” materials, they are used to offset the hardening influence of high levels of filler Can extract into process fluids, resulting in seal shrinkage & hardening Compounding: Plasticizers
21
TM H I = Original Height H D = Compressed Height H F = Recovered Height HIHI HDHD HFHF Compression Set records the amount of permanent deformation of a compressed sample over time. The Lower the Number, the Better Sealing Ability. Compression Set
22
TM High Temp Compression Set
23
TM F S = “Spring Force” FSFS Compressive Stress Relaxation records drop in “Spring Force” over time generated by a compressed rubber sample. The Higher the Number, the Better Sealing Ability. Compressive Set Relaxation
24
TM Compressive Set Relaxation
25
TM O-Ring Design Is Easy! It’s the O-Ring groove that needs special attention
26
TM What makes a reliable O-ring design? Squeeze,Seal deforms significantly (~25%),Rubber does not compress or lose volume Stretch Gland fill,Volume-to-void ratio Surface finish,Balance of machining costs with application & testing needs Installation,Protect seal from sharp edges,Provide lead-in chamfers O-Ring Design
27
TM Compression expressed as a percentage of the free-state cross-sectional thickness of the O-ring. (O-Ring C/S) - Gland Depth (O-Ring C/S) Face Seal:20-30% Static Male/Female:18-25% Reciprocating:10-20% Rotary:0-10% O-Ring Squeeze
28
TM O-Ring volume as a percentage of Gland volume. (O-Ring Volume) (Gland Volume) About 25% void space or 75% nominal fill Need space in groove to allow for volume swell, thermal expansion, and increasing width due to squeeze O-Ring Gland Fill
29
TM O-Ring Gland Fill
30
TM www.parkerorings.com www.parofluor.com Website Resources
34
TM Acknowledgements Dan Ewing, Seal Application Engineering Manager Natalie Hicks, Seal Application Engineering Manager
35
TM Patent Pending Parker IntraFlow ™ Thank You!
Similar presentations
© 2025 SlidePlayer.com. Inc.
All rights reserved.