Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32
2
Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32 Applied water pressure: day 1 to day 2: 0,1MPa day 3:0,3MPa day 4 to day 7:0,7MPa cement content CPII-E 32350kg/m³ design strength20MPa fine aggregate388kg/m³ coarse aggregate 0421kg/m³ coarse aggregate 1632kg/m² water192kg/m³ plasticiser admixture0,3% a 0,4% mc Slump90±10mm W/C ratio0,54 Penetron Admix1% of the cement content
3
Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32 - 1 week after start of water pressure
4
Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32 - 2 weeks after start of water pressure
5
Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32 - 3 weeks after start of water pressure
6
Testing of water penetration under pressure – NBR 10.787/94 (April 2007) Cement: CPII-E 32 - 4 weeks after start of water pressure