TRD Production at GSI Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005.

Similar presentations


Presentation on theme: "TRD Production at GSI Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005."— Presentation transcript:

1 TRD Production at GSI Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005

2 Overview Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - Status L5C1/L4C1 - Glue System - Testing the Properties - Summary

3 30 Radiators Frames glued 21 Radiator Frames wired 23 Padplanes glued 2 Padplanes bad Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Production Status L5C1

4 19 Moduls tested with Fe55 Source Closed with Tape Gas ArCO 2 70/30 HV-Anode 1620 V, HV-Drift -2000 V O 2 Concentration below 30ppm, Flush 40l/h, 8h up to know Dark Current < 1nA Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Testing Status L5C1

5 Finally glued Chamber 2 Modul tested with Roentgen Source Gas ArCO 2 70/30 HV-Anode 1620 V, HV-Drift -2000 V O 2 Concentration below 10ppm, Flush 40l/h, 8h up to know Dark Current < 1nA Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Testing Status L5C1

6 11 Radiators Frames glued 5 Radiator Frames wired 5 Padplanes glued Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Production Status L4C1

7 1 Moduls tested with Fe55 Source Closed with Tape Gas ArCO 2 70/30 HV-Anode 1620 V, HV-Drift -2000 V O 2 Concentration below 30ppm, Flush 40l/h, 8h up to know Dark Current < 1nA Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Testing Status L4C1

8 Problem with Glue System Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - Used Araldit AW 106/AW116 with Hardener HV953U - Sticky surface after curing time - Problem in Producing Hardener HV 953 U since 2004

9 Decision Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - Stop the TRD Production Mechanical and electrical Properties Chemical Composition was changed - Get a Charge of an modifcated Hardener to test the mech. and electr. Properties

10 Test mechanical Properties Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - cured Glue min. 24h under different climatic Conditions Shore Hardness is 60 - Observed Different Surface Quality, it depends on the Huminidity and the retention time in Air Humidity rel. 2% - 50% Temperature 23 º C – 40 º C one Sample cured in Nitrogen Atmosphere

11 Test Electrical Properties Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - under different Climatic Conditions Volume Resistivity 300 G – 8 T Ohm cm Humidity rel. 2% - 50% Temperature 23 º C – 40 º C one Sample has cured in Nitrogen Atmosphere

12 CONCLUSION Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - Orderd and distributed Hardener to finished the TRD Production - Additional Ageing Test

13 SUMMARY Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 - Delay of 6 weeks in the Production Scale - 4 L5C1and 4 L4C1 finished to shipped to HD End of October - Production Mode to build 2 TRD Chambers / 7 Working Days

14 Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005 Thank you Sandra Schwab, Anja B. Steffen Gert Augustinski, Andre Radu, Heinz W. Daues and all the Students


Download ppt "TRD Production at GSI Joerg Hehner TRD Collaboration Meeting Bucharest 26.09.2005."