1 Results of Destructive Testing Bacon Industries: LCA-4LV 3M-9882 Adhesive Tape D. Hicks10-4-01
2
2 Bacon Industries LCA-4LV Overlap Shear test of bond between Silicon and Aluminum coupon. Irradiated at University of Iowa (16 MRad)
3
3
4
4 3M-9882 Adhesive Tape Overlap Shear test of bond between two aluminum coupons. Irradiated at University of Iowa.
5
5
6
6 The radioactive source used for the samples at University of Iowa was Cesium. ASTM E 1250-88 and E 1249-93 was consulted for the testing procedure.
7
7 NEE001 Used by HERA-B; leading candidate between sensor and HDI Outgassing test: no outgassing detected Irradiation: samples sent to Iowa; most got damaged during the shipping! Wire bonding test: adhesive is soft; wire bonding using K&S 8090 a bit problematic; still working on a solution
8
8 Young’s modules important property but none of the vendors could provide this information FEA showed that this is the critical parameter in determining the stress on the epoxy. CTE has a relatively minor effect we cannot determine this easily Outside companies contacted