Presentation is loading. Please wait.

Presentation is loading. Please wait.

QUANZHOU SEASUNSTAR CRAFT CO.,LTD. Fountain Process ( Material: Polyresin )

Similar presentations


Presentation on theme: "QUANZHOU SEASUNSTAR CRAFT CO.,LTD. Fountain Process ( Material: Polyresin )"— Presentation transcript:

1 QUANZHOU SEASUNSTAR CRAFT CO.,LTD. Fountain Process ( Material: Polyresin )

2 Drawing Design:

3 Carving: → The new sculptures are generally based on the drawing designs. Material: Black mud, Gesso →

4 Carving: Sometimes,our engineers finish the new sculpture according to some material, things such as bark, wood,stone,animal etc. ← ↙ The board and bucket are made of gesso. The pipe is real, not sculptural. → ↑ The base and shoes are made of black mud. It makes the sculpture more natural than using gesso.

5 Opening Mold: The mold sample →→ ↓ Pour the slurry of Silica gel and brush. ← ← Paste the fiberglass on the mold sample. Material: Polyfoam, The slurry of silica gel,The slurry of polyresin, Yellow mud,Fiberglass.

6 Opening Mold: Pour, brush and paste again. →→ ↓ ← Then brush the slurry of polyresin.

7 Remove the partial polyfoam.Repeat the above steps. Opening Mold: → → The mold is OK.

8 Shaping : → One mold consists of two parts. Join the two parts of the mold. ← Material: Slurry of Poly resin Check the mold and make sure the mold is good for production → Fix two parts tight with screws. ○

9 → Pour the slurry of poly resin into the mold ○ Roll the mold to make the slurry cover the whole silica mold. Shaping : → After rolling, need 15 minutes for the slurry to solidify. Open the mold and remove the silica mold from the shaped product → → Shaped product

10 Grinding,Drilling and Trimming: → ←

11 Washing and Steeping : →

12 Mending: Makes the mold line smooth and natural after trimming.

13 Mending: Before MendingAfter Mending

14 Painting: Spraying

15 Painting: Brushing

16 Testing: (1) Water leakage test(2) Function testing

17 Testing: \ □ Use paper to test the splash. If splash is too much, test fail, then product needs to be re-worked. ( Dry paper ) (Testing time: 24 hours) Water flow testing

18 Testing: The good testing. □ ← Water flow testing

19 Packaging: → □ □ Pump/Transformer Instruction manual Place the Pump , Transformer , Product Instruction in related space. → →


Download ppt "QUANZHOU SEASUNSTAR CRAFT CO.,LTD. Fountain Process ( Material: Polyresin )"